Summer arrived, hot melt marking paint matters
 Release Time:2018-07-25 | Visits:

At present, China's industry standard stipulates that the softening point of hot-melt marking coating is 90-125 degree softening point, which is a qualified coating. In the summer of 2017, the ground temperature is up to 75 degrees centigrade. If your marking paint is about 90 degrees soft, there will be a lot of problems.


1. Poor anti fouling and easy to blacken

2. The glass bead is all pressed into the interior of the marking line

3. Poor wear resistance,

4. The thickness of the marking line is not up to standard

5. Shedding of glass beads

6, the marking line is not reflected


Therefore, in summer, the temperature is high and the marking is soft.


Choose the right raw material and improve the marking hardness without losing the toughness.

WECHAT

Service HotLine
+86-18612008875
Copyright© 2018 Beijing Jingyi Technology Co., Ltd. All Rights Reserved 京ICP备18037854号

ON
LINE

HOT
LINE

18612008875 13683286371
SERVICE LINE

LINE
QQ

Online QQ consultation Click here to send me a message

OUR
WECH

Follow the official WeChat
TOP